PROBLEM TO BE SOLVED: To provide a reduction powder capable of quickly making a variety of oxidized substances into a reduced condition simply even in any place, and a method of producing the same.SOLUTION: Specifically, a reduction powder mainly includes five kinds of metals of iron, zinc, magnesium, copper and potassium. The main metals and metals including calcium, molybdenum, vanadium, nickel, manganese, selenium, sodium, cobalt, lithium, phosphorus, and chromium are ground into a metal powder having a granularity of about 100 mesh. An ionized mixture is obtained by mixing the metal powder, an oxidized substance and a salt. The reduction powder includes an oxidized powder having a granularity within a range of 100-3,000 mesh and differing in a granularity in a stepwise fashion obtained by shaving the surface of a soft solid obtained by putting the ionized mixture into a mold frame and leaving it to stand, and thereafter removing the mold frame.COPYRIGHT: (C)2014,JPO&INPIT【課題】本発明の目的は、様々な酸化物質を簡便に、且つ、どのような場所であっても素早く還元状態にすることができる還元パウダー及びその製造方法を提供することである。【解決手段】本発明の還元パウダーは、具体的には、本発明に係る還元パウダーは、鉄・亜鉛・マグネシウム・銅・カリウムの5種の金属を主体とし、該主体金属と、カルシウム・モリブデン・バナジウム・ニッケル・マンガン・セレニウム・ナトリウム・コバルト・リチウム・リン・クロムから成る金属を、それぞれ100メッシュ程度の金属粉にし、該金属粉と酸性物質と塩を混合してイオン化混合体を作り、それを型枠に入れて放置した後、前記型枠を取り外すことにより得られるやわらかい固体の表面を削って、細かさを100~3000メッシュの範囲で且つ該細かさを段階的に異ならせた酸化粉体から成る。【選択図】図1