Producing an elastic film, comprises pre-mixing the polymer components to produce a polymer composition containing styrene block copolymers, and extruding the polymer composition to obtain at least one layer, where zeolite is added during pre-mixing and/or extrusion. The pore opening of zeolite is greater than 2.5 Å and less than 5.5 Å .