PROBLEM TO BE SOLVED: To obtain an aqueous gel composition without exposing additives to the aqueous gel composition such as a perfume to high temperatures.SOLUTION: The method for manufacturing the aqueous gel composition comprises a gelling agent-dissolving step of mixing a mixture of copolymers of n=1-10 represented by chemical formula 1: CH3(CH2)9CH(C12H25)CH2-O-(CH2CH2O)20-CONH-(CH2)6-NHCO-[O-(CH2CH2O)240-CONH(CH2)6NHCO]n-(OCH2CH2)20-O-CH2(C12H25)CH(CH2)9CH3 as a gelling agent and water and a water soluble alcohol as solvent for dissolving the gelling agent to dissolve the gelling agent in the solvents and obtain a gelling agent solution and a gelling step of adding water to the gelling agent solution to effect gelling, and between the gelling agent-dissolving step and the gelling step or in the gelling step, additives for the aqueous gel composition are added and mixed into the gelling agent solution of room temperature so as to uniformly disperse the additives into the gelling agent solution.COPYRIGHT: (C)2010,JPO&INPIT【課題】香料等の水性ゲル状組成物への添加物を高温に晒すことなく、水性ゲル状組成物を得る。【解決手段】ゲル化剤として化学式1で表されるn=1~10のコポリマーの混合物と、ゲル化剤を溶解する溶剤として水及び水溶性アルコール類とを混合し、ゲル化剤を溶剤に溶解させてゲル化剤溶解液を得るゲル化剤溶解工程と、ゲル化剤溶解液に水を加えてゲル化するゲル化工程とを含み、ゲル化剤溶解工程とゲル化工程との間またはゲル化工程で、室温のゲル化剤溶解液に対して水性ゲル状組成物への添加物を添加し混合してゲル化剤溶解液に均一に分散させるようにした。<化1>CH3(CH2)9CH(C12H25)CH2-O-(CH2CH2O)20-CONH-(CH2)6-NHCO-[O-(CH2CH2O)240-CONH(CH2)6NHCO]n-(OCH2CH2)20-O-CH2(C12H25)CH(CH2)9CH3【選択図】なし