Provided is a process for forming a personal care article comprising producing a personal care article from a twin screw extruder employing blowing agents, the personal care article including (i) from about 10% to about 60% of one or more anionic surfactants, wherein the one or more anionic surfactants have a Krafft point of less than about 30°C (ii) from about 10% to about 50% of one or more water soluble polymers (iii) from about 1% to about 30% of one or more plasticizers and (iv) from about 0.01% to about 40% water. The personal care article has a density of from about 0.05 g/cm3 to about 0.95 g/cm3.La présente invention concerne un procédé pour former un article de soin personnel comprenant la production dun article de soin personnel à partir dune extrudeuse à deux vis au moyen dagents soufflants, larticle de soin personnel comprenant (i) denviron 10 % à environ 60 % dun ou plusieurs tensioactifs anioniques, les un ou plusieurs tensioactifs anioniques ayant un point de Krafft inférieur à environ 30 °C (ii) denviron 10 % à environ 50 % dun ou plusieurs polymères hydrosolubles (iii) denviron 1 % à environ 30 % dun ou plusieurs plastifiants et (iv) denviron 0,01 % à environ 40 % deau. Larticle de soin personnel a une masse volumique denviron 0,05 g/cm3 à environ 0,95 g/cm3.