A method for producing a sterilized medical molded body by high energy irradiation of the medical molded body with an exposure dose E, the medical molded body being formed from a resin composition comprising: 100 parts by weight of a block copolymer hydride in which 99% or more of the total unsaturated bond of a block copolymer is hydrogenated, the block copolymer comprising a polymer block (A) that is composed mainly of a unit derived from an aromatic vinyl compound and a polymer block (B) that is composed mainly of a unit derived from a chain conjugated diene compound with a ratio of the weight fraction of the polymer block (A) and the polymer block (B) being 30:70 to 70:30 and a phenolic antioxidant in an amount of parts by weight represented by formula 1: W=[0.46×(100-H)+0.04]×(E/25) (In the formula, W is the parts by weight of the antioxidant with respect to 100 parts by weight of the block copolymer hydride, H is a hydrogenation degree of the block copolymer hydride indicated in % units, H is a numerical value of 99 to 100, and E is an exposure dose of high energy rays indicated in kGy units) or more and 0.50 parts by weight or less.Linvention concerne un procédé de production dun corps moulé médical stérilisé par irradiation à haute énergie du corps moulé médical avec une dose dexposition E, le corps moulé médical se composant dune composition de résine comprenant : 100 parties en poids dun complexe copolymère séquencé-hydrure dans lequel 99 % ou plus de la liaison insaturée totale dun copolymère séquencé sont hydrogénés, le copolymère séquencé comprenant une séquence polymère (A) qui est composée principalement dun motif dérivé dun composé vinylique aromatique et une séquence polymère (B) qui est composée principalement dun motif dérivé dun composé diénique conjugué à chaîne, un rapport de la fraction pondérale de la séquence polymère (A) et de la séquence polymère (B) allant de 30:70 à 70:30 et un antioxydant phénolique en une quantité de parties en poids