The present invention provides an artificial reef fabrication method comprising the steps of: (a) manufacturing a fiber-reinforced plastic or synthetic resin molded body having an opening formed through a surface thereof and having a containing space formed therein; (b) filling the containing space with a reinforcement material; and (c) sealing the opening with the fiber-reinforced plastic or synthetic resin. According to the artificial reef fabrication method of the present invention, a fiber-reinforced plastic or synthetic resin molded body is filled with a concrete reinforcement material and is sealed with fiber-reinforced plastic or synthetic resin; accordingly, the concrete reinforcement material is not exposed to the outside, and no alkaline material is eluted to seawater, thereby providing strong durability against salt; and the surface of the fiber-reinforced plastic or synthetic resin is coated with stone powder or ceramic powder such that seaweed can easily root thereon, making it possible to fabricate an artificial reef on which a submerged forest can easily develop.La présente invention concerne un procédé de fabrication d'un récif artificiel comprenant les étapes consistant à : (a) fabriquer un corps moulé en plastique ou en résine synthétique renforcé(e) par des fibres présentant une ouverture formée à travers une surface correspondante et présentant un espace de confinement formé en son sein ; (b) remplir l'espace de confinement par un matériau de renforcement ; et (c) fermer hermétiquement l'ouverture par le plastique ou la résine synthétique renforcé(e) par des fibres. Selon le procédé de fabrication d'un récif artificiel de la présente invention, un corps moulé en plastique ou en résine synthétique renforcé(e) par des fibres est rempli d'un matériau de renforcement en béton et est fermé hermétiquement par un plastique ou une résine synthétique renforcé(e) par des fibres ; par conséquent, le matériau de renforcement en béton n'est pas apparent à l'e