PROBLEM TO BE SOLVED: To provide a coating material that is applied to a denture base used by patients with xerostomia to give an appropriate level of moisture and the moistness can be retained for at least one week (high durability).SOLUTION: A non-crosslinking copolymer comprising both of a polymer block formed from a hydrophilic monomer and a polymer block formed from a hydrophobic monomer and is insoluble in water is dissolved in a volatile organic solvent and the solution is used as a coating material. As this copolymer, particularly is cited a block copomer or graft copolymer from a polymer represented by the formula (1) (wherein R1 and R2 are each independently H or methyl and n is an integer of 1 to 10) and poly(methyl methacrylate) polymer.COPYRIGHT: (C)2006,JPO&NCIPI【課題】口腔乾燥症患者が用いている義歯床に、適度な保湿性を与え、かつ少なくとも1週間以上はその効果が持続する(耐久性に優れる)コーティング材を得る。【解決手段】親水性単量体に基づくポリマーブロックと、疎水性単量体に基づくポリマーブロックとの双方を有し、かつ水に対して不溶である非架橋の共重合体を、揮発性有機溶媒に溶解した溶液をコーティング材とする。この共重合体としては、下記式(1)【化1】(但し、R1、R2は各々独立に水素原子またはメチル基を示し、nは1~10の整数)で表される重合体と、メチルメタクリレートとのブロック共重合体又はグラフト共重合体が特に好ましい。【選択図】 なし