The invention copolymerizing monomer components comprising a vinyl monomer having a crosslinkable vinyl monomer and a heterocyclic aromatic ring the BET specific surface area obtained by 10 / g or higher initiates the deodorant particle . In addition, also disclosed deodorant particles containing the metal ion . A monomer component containing a vinyl monomer having a crosslinkable vinyl monomer and a heterocyclic aromatic ring , water type and the absolute value of the solubility parameter difference by using 0 to 2.0, the organic solvent of the monomer component ( ) suspension polymerization or precipitation discloses a process of the deodorant particles with the step of performing the polymerization . In addition , by contacting the solvent dissolving the metal salt and the particle obtained by the polymerization , initiates the process of the deodorant particles with the step of carrying the metal ions to particles .본 발명은 가교성 비닐모노머 및 헤테로방향고리를 가지는 비닐모노머를 포함하는 모노머 성분을 공중합하여 얻어지는 BET 비표면적이 10㎡/g 이상인 소취 입자를 개시한다. 또한 금속 이온을 함유하는 소취 입자도 개시한다. 가교성 비닐모노머 및 헤테로방향고리를 가지는 비닐모노머를 포함하는 모노머 성분을, 모노머 성분과의 용해도 파라미터 차의 절대값이 0~2.0인 유기용제를 사용하여 수중유형(水中油型) 현탁중합 또는 침전중합을 행하는 공정을 가지는 소취 입자의 제조법을 개시한다. 또한, 중합에 의해 얻어진 입자와 금속염을 용해시킨 용제를 접촉시켜, 입자에 금속 이온을 담지시키는 공정을 가지는 소취 입자의 제조법을 개시한다.