FIELD: chemistry.SUBSTANCE: water-absorbing polymer particles are described, the polymer particles having average sphericity of at least 0.84, content of hydrophobic solvent of less than 0.005 wt % and permeability of at least 5×10-7 cm3s/g and contain polyatomic cations. Also described is a method of obtaining said water-absorbing polymer particles by polymerising droplets of a monomer solution containing a) at least one ethylenically unsaturated monomer having acid groups, b) at least one cross-linking agent, c) at least one initiator, d) water in the gas phase surrounding the droplets, characterised by that the monomer solution contains polyatomic cations and the polymer particles have average diameter of at least 150 mcm, wherein the number of polyatomic cations is selected such that neither clouding nor precipitation occurs in the monomer solution and, if needed, the process is carried out in the presence of a hydrophobic solvent. Use of said particles to obtain sanitary and hygiene products is also described.EFFECT: obtaining water-absorbing particles with high permeability.19 cl, 1 tbl, 4 exНастоящее изобретение относится к способу получения водопоглощающих полимерных частиц. Описаны водопоглощающие полимерные частицы, причем полимерные частицы имеют среднюю сферичность, по меньшей мере, 0,84, содержание гидрофобного растворителя меньше чем 0,005 мас.%, проницаемость, по меньшей мере, 5×10-7 см3 c/г и содержат многоатомные катионы. Также описан способ получения указанных выше водопоглощающих полимерных частиц путем полимеризации капель мономерного раствора, содержащего а) по меньшей мере, один этилен-ненасыщенный мономер, имеющий кислотные группы, b) по меньшей мере, один сшиватель, с) по меньшей мере, один инициатор, d) воду, в окружающей капли газовой фазе, отличающийся тем, что мономерный раствор содержит многоатомные катионы и полимерные частицы имеют средний диаметр, по меньшей мере, 150 мкм, причем количество многоатомного катиона выбирают таким образом