A tip rod made of a fiber reinforced resin has a solid structure at least at its distal end portion. The tip rod is formed by dispersing reinforcement fibers in a matrix resin, molding the matrix resin that contains the reinforcement fibers into a prescribed shape, and heating the molded matrix resin that contains the reinforcement fibers to be cured. An average diameter of the reinforcement fibers is 3 to 15 μm, an average length of the reinforcement fibers is 0.5 to 10 mm, a content of the fibers dispersed in the matrix resin is 3 to 50 wt %. The solid structure of the tip rod includes an outer layer, an intermediate layer, and an inner layer in which the reinforcement fibers are directed in a different direction for each layer. Alternatively the structure may include the outer layer and the inner layer.