摘要:
PROBLEM TO BE SOLVED: To provide a film for a package excellent in scratch resistance, impact resistance and the visibility of a content, and also excellent in easy openability.SOLUTION: Provided is a film 1 for a package comprising: a base material layer 10 having vapor barrier properties and oxygen barrier properties a sealant layer 20 and an adhesive layer 30 arranged between the base material layer 10 and the sealant layer 20, the base material layer 10 includes a layer of inorganic vapor-deposited nylon and a layer of biaxial drawing polypropylene on the surface, the thickness of the adhesive layer 30 is 4.0 μm or lower, the thickness of the sealant layer 20 is 30 to 80 μm, the adhesive strength between the base material layer 10 and the sealant layer 20 is 3N/15 mm or higher, and a water vapor permeation degree is 0.7 to 3.0 g/m2.SELECTED DRAWING: Figure 1COPYRIGHT: (C)2017,JPO&INPIT【課題】耐スクラッチ性、耐衝撃性、内容物の視認性に優れ、かつ、易開封性に優れる包装体用フィルム。【解決手段】水蒸気バリア性及び酸素バリア性を有する基材層10と、シーラント層20と、前記基材層10と前記シーラント層20との間に配された接着層30と、を備え、前記基材層10は、無機蒸着ナイロンの層又は二軸延伸ポリプロピレンの層を表面に備え、前記接着層30の厚さは4.0μm以下であり、前記シーラント層20の厚さは30~80μmであり、前記基材層10と前記シーラント層20との接着強度は3N/15mm以上であり、水蒸気透過度が0.7~3.0g/m2である、包装体用フィルム1。【選択図】図1
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充