摘要:
PROBLEM TO BE SOLVED: To provide a method for manufacturing a fastening tape that is hardly torn off when being put on or worn while the flexibility is maintained.SOLUTION: The method for manufacturing the fastening tape includes: a placing step of placing a belt-like long hook material 13 on a part of one surface of a long base material sheet 11 along the longitudinal direction thereof to obtain a laminate 15 a reinforcement joining step of joining, after the laminate 15 obtained, the long base material sheet 11 and the long hook material 13, and then, pressing an area other than the area on which the long hook member 13 is placed to thereby form a recess for reinforcement to obtain a joined body 16 and a cutting step of cutting and separating the joined body 16 into a predetermined size to obtain a plurality of fastening tapes 10a.COPYRIGHT: (C)2013,JPO&INPIT【課題】柔軟性を維持しつつ、着用する際または着用中に、千切れ難い止着テープを製造することが可能な止着テープの製造方法を提供する。【解決手段】長尺基材シート11の一方の面の一部に、その長手方向に沿って帯状の長尺フック材13を載置して積層体15を得る載置工程と、積層体15を得た後、長尺基材シート11と長尺フック材13を接合し、その後、長尺フック材13を載置した領域以外の領域を押圧することにより補強用凹部を形成して接合体16を得る補強接合工程と、接合体16を所定の大きさに切り離して複数の止着テープ10aを得る切断工程と、を備えた止着テープの製造方法。【選択図】図22
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充