A process for producing an absorbent resin in which water-soluble ethylenically unsaturated monomers to which an internal cross-linking agent is added are used to coagulate primary particles obtained by reverse-phase suspension polymerization at the first stage by reverse-phase suspension polymerization at the second stage, The addition amount of the internal cross-linking agent is A mole relative to 100 moles of the water-soluble ethylenic unsaturated monomer used in the first stage, and the addition amount of the internal cross-linking agent in the second row is set to B mole based on 100 moles of the water-soluble ethylenic unsaturated monomer used in the second-If A and B satisfy A < = 5.0 x 10 <-3, And further satisfies 2 B / A 10.By the manufacturing method according to the present invention, it is possible to provide an absorbent resin having excellent liquid passing performance, an absorbent containing it, and an absorbent article.내부 가교제가 첨가된 수용성 에틸렌성 불포화 단량체를 사용하여, 제 1 단째의 역상 현탁 중합에 의해 얻어진 1 차 입자를 제 2 단째의 역상 현탁 중합에 의해 응집시키는 흡수성 수지의 제조 방법으로서, 제 1 단째의 내부 가교제의 첨가량을 제 1 단째에 사용되는 수용성 에틸렌성 불포화 단량체 100 몰에 대하여 A 몰, 및 제 2 단째의 내부 가교제의 첨가량을 제 2 단째에 사용되는 수용성 에틸렌성 불포화 단량체 100 몰에 대하여 B 몰로 한 경우, A 및 B 가 A ≤ 5.0 × 10-3, 또한 2 ≤ B/A ≤ 10 의 관계를 만족하는 것을 특징으로 하는 흡수성 수지의 제조 방법.본 발명에 관련된 제조 방법에 의해, 통액 성능이 우수한 흡수성 수지, 그것을 포함하는 흡수체 및 흡수성 물품을 제공할 수 있다.