您的位置: 首页 > 农业专利 > 详情页

線形弾性変形をし、超高強度、超低弾性特性を有するチタン合金
专利权人:
韓国機械材料技術院
发明人:
パク チャンヘ,ヨム ジョンテク,キム スンオン,キム スンウン,キム ジョンハン,ホン ジャケン
申请号:
JP2015521528
公开号:
JP6006872B2
申请日:
2013.03.28
申请国别(地区):
JP
年份:
2016
代理人:
摘要:
high strength, in the composition of the titanium alloy having a low modulus of elasticity, the structure of the titanium alloy, titanium (Ti), niobium (Nb), zirconium (Zr), containing iron (Fe) and oxygen (O), respectively at a predetermined ratio and the linear elastic deformation, ultra-high strength, the titanium alloy having a ultra-low elastic properties ( Ti-20Nb-5Zr-1Fe-O) it provides. Is a linear elastic deformation having the above composition, ultra-high strength, the titanium of the titanium alloy having a ultra-low elastic properties (Ti-20Nb-5Zr-1Fe-O) (Ti), niobium (Nb), zirconium (Zr), iron (Fe) and component ratio of oxygen (O) is, niobium (Nb) 18 ~ 22at.%, zirconium (Zr) 3~7 at.%, iron (Fe) 0.5~3.0 at.%, oxygen (O) 0.1 ~1.0 wt.%, and characterized in that it the balance titanium (Ti).BACKGROUND 1高強度、低弾性係数を有するチタン合金の組成において、前記チタン合金の構成は、チタン(Ti)、ニオブ(Nb)、ジルコニウム(Zr)、鉄(Fe)及び酸素(O)をそれぞれ所定の比率で含む、線形弾性変形をし、超高強度、超低弾性特性を有するチタン合金(Ti-20Nb-5Zr-1Fe-O)を提供する。上記組成からなる線形弾性変形をし、超高強度、超低弾性特性を有するチタン合金(Ti-20Nb-5Zr-1Fe-O)のチタン(Ti)、ニオブ(Nb)、ジルコニウム(Zr)、鉄(Fe)及び酸素(O)の構成比率は、ニオブ(Nb)18 ~ 22at.%、ジルコニウム(Zr)3~7 at.%、鉄(Fe)0.5~3.0 at.%、酸素(O)0.1~1.0 wt.%、及び残部チタン(Ti)からなることを特徴とする。【選択図】図1
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充