PARTICULES DE RÉSINE ABSORBANT L'EAU, PROCÉDÉ POUR LA FABRICATION DE PARTICULES DE RÉSINE ABSORBANT L'EAU, CORPS D'ABSORPTION, ARTICLE ABSORBANT ET MATÉRIAU D'ÉTANCHÉITÉ À L'EAU
Disclosed is a water-absorbent resin particle in which the water-absorption rate of physiological saline is 1 second to 15 seconds, the median particle size is 100 µm to 600 µm, and the residual volatile component content is 1.5% by weight or less.