U&I CORPORATION;KOREA INSTITUTE OF SCIENCE AND TECHNOLOGY
发明人:
구자교,정화철,심원현,노형진,석현광,김유찬,KOO JA KYO,HWA CHUL JUNG,WON HYUN SHIM,HYUNG JIN ROH,SEOK HYUN KWANG,KIM YU CHAN
申请号:
KR1020190118726
公开号:
KR1020541910000B1
申请日:
2019.09.26
申请国别(地区):
KR
年份:
2020
代理人:
摘要:
A biodegradable metal alloy, at least 0.05% by weight and less than 0.15% by weight of calcium; A metal element X having a hexagonal dense structure (HCP) and at least one selected from the group consisting of Sc, Gd, Dy, Y, and Zn; And a residual amount of magnesium, wherein the metal element X has a solubility in magnesium of at least 5%, and is dissolved in magnesium to form a separate precipitated phase, and the metal element X is 0.1 in the total biodegradable metal alloy. There is provided a biodegradable metal alloy, characterized in that the content of more than 1% by weight.생체분해성 금속 합금으로, 0.05중량% 이상 0.15 중량% 미만의 칼슘; 육방조밀구조(HCP)를 가지며, Sc, Gd, Dy, Y, 및 Zn로 이루어진 군으로부터 선택된 적어도 어느 하나인 금속원소 X; 및 잔량의 마그네슘을 포함하며, 상기 금속원소 X는 마그네슘에 대한 고용도는 5% 이상이며, 상기 마그네슘에 고용되어 별도의 석출상을 형성하지 않으며, 상기 금속 원소 X는 전체 생체분해성 금속 합금 중 0.1 이상 1 중량% 이하의 함량인 것을 특징으로 하는 생체분해성 금속 합금이 제공된다.