The ultraviolet cured optic binder has low curing shrinkage, low hardness and high optical transmittance. Technology programs are as follows: an ultraviolet cured optic binder composition includes the following raw material in parts by weight: 50 to 100 parts of prepolymer, 20 to 90 parts of inert resin, 35 to 70 parts of monomer, 5 to 12 parts of photoinitiator, 2 to 3 parts of coupling reagent, 1 to 2 parts of auxiliaries.