歯牙石灰化剤及びその製造方法
专利权人:
クラレノリタケデンタル株式会社
发明人:
橋本 正,石原 周明,尾下 瑞子
申请号:
JP2013536321
公开号:
JPWO2013047558A1
申请日:
2012.09.26
申请国别(地区):
JP
年份:
2015
代理人:
摘要:
poorly soluble acidic calcium phosphate particles (A), an alkali metal salt of phosphoric acid (B) and there is provided a tooth calcification agent containing water (C), poorly soluble acidic calcium phosphate particles (A) is, calcium hydrogen phosphate anhydrous [CaHPO4] particles, tricalcium phosphate [Ca3 (PO4) 2] particles , calcium pyrophosphate [Ca2P2O7] particles, phosphoric acid eight calcium pentahydrate [Ca8H2 (PO4) 6 5H2O] particles, calcium dihydrate [Ca2P2O7 2H2O] particle pyrophosphate, and calcium hydrogen phosphate dihydrate [CaHPO4 2H2O] is at least one selected from the group consisting of particles, 15 to 80 parts by weight of hardly soluble acidic calcium phosphate particles (A) relative to the total amount 100 parts by weight of the tooth Fang calcification agents, and water ( C) The containing 15-84 parts by weight, and the amount of the alkali metal salt (B) of the phosphoric acid to 100 parts by weight of hardly soluble acidic calcium phosphate particles (A) is characterized in that a 0.1 to 80 parts by weight . Thus, highly calcified effective tooth calcification agent.難溶性酸性リン酸カルシウム粒子(A)、リン酸のアルカリ金属塩(B)、及び水(C)を含有する歯牙石灰化剤であって、難溶性酸性リン酸カルシウム粒子(A)が、無水リン酸一水素カルシウム[CaHPO4]粒子、リン酸三カルシウム[Ca3(PO4)2]粒子、ピロリン酸カルシウム[Ca2P2O7]粒子、リン酸八カルシウム5水和物[Ca8H2(PO4)6・5H2O]粒子、ピロリン酸カルシウム2水和物[Ca2P2O7・2H2O]粒子、及びリン酸一水素カルシウム2水和物[CaHPO4・2H2O]粒子からなる群から選択される少なくとも1種であり、該歯牙石灰化剤の全量100重量部に対して難溶性酸性リン酸カルシウム粒子(A)を15~80重量部、及び水(C)を15~84重量部含み、かつ難溶性酸性リン酸カルシウム粒子(A)100重量部に対するリン酸のアルカリ金属塩(B)の配合量が0.1~80重量部であることを特徴とする。これにより、石灰化効果の高い歯牙石灰化剤が提供される。
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充