PROBLEM TO BE SOLVED: To provide a new gelling composition capable of facilitating, for example, a dispensing operation or a mixing operation with other components for a solution obtained by adding water to a gelling composition. And According to the present invention, for example, a gelling composition that requires a metal ion for gelation and is used by transferring from a sol state to a gel state at room temperature without adding water and performing heating and cooling operations. The sol solution prepared by adding water to the gelled composition, after hydration, maintains the sol state for at least 90 seconds in the presence of metal ions, and has a viscosity of 1 minute after hydration for 1 minute after hydration. A delayed gelling composition characterized by reaching a viscosity of 2 to 1.5 times and exhibiting a gel state within 6 hours after hydration can be mentioned. [Selection diagram] None【課題】ゲル化組成物に水を加えた溶液に対して、例えば分注操作や他の成分との混合操作を容易にすることができる新たなゲル化組成物を提供することを主な課題とする。【解決手段】本発明として、例えば、ゲル化に金属イオンを必要とし、水を加え加温冷却操作を行うことなく常温でゾル状態からゲル状態に転移させて使用するゲル化組成物であって、かかるゲル化組成物に水を加えたゾル溶液は、加水後、金属イオンの存在下において少なくとも90秒間ゾル状態を持続し、加水後1時間までに加水後1分の粘度に対して1.2~1.5倍の粘度に達し、加水後6時間までにゲル状態を呈することを特徴とする遅延性ゲル化組成物を挙げることができる。【選択図】なし