Scan posts for planning and manufacturing systems of oral or maxillofacial restoration products are provided. The scan post comprises a body made of titanium or stainless steel and at least a portion of the surface of the body is surface treated using the following steps which are performed to obtain a surface roughness Ra of about 1.5 [ Sandblasting the exposed surface and coating the treated surface using a physical vapor deposition (PVD) or chemical vapor deposition (CVD) process. The coating deposits on the treated surface one layer of the group consisting of chromium, chromium nitride, aluminum nitride and titanium nitride. The surface treatment may include an intermediate step of rinsing the body with acid to remove sand residue from the scan post, before and after the sandblasting step.구강 또는 위턱얼굴(maxillofacial) 복원 제품의 계획 및 제조 시스템용 스캔 포스트가 제공된다. 스캔 포스트는 티타늄 또는 스테인리스 스틸로 제조된 본체를 포함하고, 본체의 표면의 적어도 일부는 이하의 단계를 이용하여 표면 처리되며, 이러한 단계는, 약 1.5㎛ 내지 2.5㎛의 표면 조도 Ra를 얻기 위해 처리된 표면을 샌드 블래스팅하는 단계와, 물리 기상 증착(PVD) 또는 화학 기상 증착(CVD) 프로세스를 이용하여 처리된 표면을 코팅하는 단계를 포함한다. 코팅은 처리된 표면 상에, 크롬, 질화크롬, 질화알루미늄 및 질화티타늄으로 구성된 군 중 하나의 층을 증착한다. 표면 처리는 샌드 블래스팅하는 단계 후 및 코팅하는 단계 전에, 스캔 포스트로부터 샌드 잔여물을 제거하기 위해 본체를 산으로 헹구는 중간 단계를 포함할 수 있다.