The present invention relates to an absorbent article (10; 20; 30) comprising a liquid permeable topsheet (102; 202), a liquid-impermeable backsheet (103; 203; 303) and an absorbent core (104; 204; 304) positioned between the topsheet (102; 202) and the backsheet (103; 203; 303). The absorbent article comprises pressure sensitive adhesive on a garment facing surface of the backsheet (103; 203; 303), and the back sheet (103; 203; 303) is a breathable polyolefin-based film and has a Water Vapour Transmission Rate measured according to NWSP 070.4.RO (15) of at least 1000 g/m2/24h, preferably at least 3000 g/m2/24h, and a tear resistance measured according to Elmendorf Tear ASTM D1922 (15) of at least 300 mN.La presente invención se refiere a un artículo absorbente (10; 20; 30) que comprende una hoja superior permeable a líquido (102; 202), una hoja posterior impermeable a líquido (103; 203; 303) y un núcleo absorbente (104; 204; 304) posicionado entre la hoja superior (102; 202) y la hoja posterior (103; 203; 303). El artículo absorbente comprende adhesivo sensible a presión en una superficie orientada a la prenda de la hoja posterior (103; 203; 303), y la hoja posterior (103; 203; 303) es una película a base de poliolefina transpirable y tiene una Velocidad de Transmisión de Vapor de Agua medida de acuerdo a NWSP 070.4.RO (15) de al menos 1000 g/m2/24h, preferentemente al menos 3000 g/m2/24h, y una resistencia a rompimiento medida de acuerdo a ASTM D1922 de Rompimiento Elmendorf (15) de al menos 300 mN.