PROBLEM TO BE SOLVED: To provide a glass tube semi-finished product or a hollow glass product manufactured from the glass tube semi-finished product.SOLUTION: One embodiment is provided with a first marking containing information regarding origin of a glass tube semi-finished product or information regarding origin and manufacture of the glass tube semi-finished product, and a second marking containing information linked to the information in the first marking, so as to allow determination to be made about originality, particularly authenticity, or to allow determination to be made about origin of the glass tube semi-finished product and/or origin of an apparatus with which the first and/or second marking is generated on the glass tube semi-finished product. Advantageously, the first marking is a marking that is produced at a temperatures above a transformation temperature of the glass in a counterfeit-proof manner. A combination of two markings provides a high level of protection against counterfeiting.SELECTED DRAWING: Figure 6bCOPYRIGHT: (C)2018,JPO&INPIT【課題】ガラス管半製品またはガラス管半製品から製造された中空ガラス製品である。【解決手段】ガラス管半製品の原物に関する情報、またはガラス管半製品の原物および製造に関する情報を含んでいる第1のマーキングと、第2のマーキングであって、オリジナリティ、特に真正性を判断できるようにするために、またはガラス管半製品の原物および/またはガラス管半製品に第1のマーキングおよび/または第2のマーキングを形成した装置の原物を判断できるようにするために、第1のマーキングの情報にリンクされている情報を含んでいる第2のマーキングと、が設けられている。有利には、第1のマーキングは、偽造が防止されるように、ガラスの転移温度を上回る温度で形成されたマーキングである。2つのマーキングの組合せは、偽造に対する高いレベルの保護を提供する。【選択図】図6b