An objective of the present invention is to provide a method of manufacturing a Ni-Ti file for precise endodontic treatment which is capable of minimizing an error of super-elastic modification or concentricity of an Ni-Ti wire when a grinding work is performed. According to a method of manufacturing a Ni-Ti file for precise endodontic treatment of the present invention, a flute of the Ni-Ti wire is ground while an outer surface of the Ni-Ti wire post-processed into a taper shape is supported by a jig in state that a section of the Ni-Ti wire of which the flute is ground is clamped. Specifically, the stress of the wire surface can be removed through electrolytic polishing and heat treatment after grinding the flute and the dental pulp removed by improving the lubricity can be exhausted to an outside of teeth.본 발명은 Ni-Ti 와이어의 플루트를 연삭할 와이어 구간을 클램핑한 상태나 테이퍼 형태로 미리 가공한 Ni-Ti 와이어의 외주면을 지그로 지지한 상태에서 플루트를 연삭하여 가공함으로써, 연삭 가공할 때 Ni-Ti 와이의 초탄성 변형이나 동심도(同心度)의 오차를 최소화하여 정밀한 근관 치료용 Ni-Ti 파일을 얻는 제조방법을 제공하는 데 그 목적이 있다.특히, 본 발명은 플루트를 연삭한 다음에 전해 연마와 열처리를 통해 와이어 표면의 응력 제거와 윤활성을 향상하여 제거한 치수를 치아 외부로 쉽게 배출할 수 있게 한 근관 치료용 Ni-Ti 파일의 제조방법을 제공하는 데 다른 목적이 있다.