A method of manufacturing a needle includes diluting a lubricant, that is biocompatible and soluble in a solvent, with a solvent, that includes one of an aliphatic hydrocarbon, an aromatic hydrocarbon and a chlorinated solvent mixing the lubricant and the solvent to obtain a coating and inserting a needle into a container housing the coating. The needle may include a hollow tube. When the needle is inserted into the container housing the coating, at least a portion of the hollow tube may be covered with the coating. A needle for reducing a force during insertion in a body includes a hollow tube configured to enter a body and a coating coupled to at least a portion of the hollow tube. The coating comprises a lubricant that is biocompatible and is soluble in a solvent and a solvent including one of an aliphatic hydrocarbon, an aromatic hydrocarbon and a chlorinated solvent.linvention concerne Un procédé de fabrication dune aiguille, ledit procédé comprenant la dilution dun lubrifiant, qui est biocompatible et soluble dans un solvant, avec un solvant, qui comporte lun parmi un hydrocarbure aliphatique, un hydrocarbure aromatique et un solvant chloré le mélange du lubrifiant et du solvant pour obtenir un revêtement et linsertion dune aiguille dans un récipient logeant le revêtement. Laiguille peut comporter un tube creux. Une aiguille permettant de réduire une force pendant linsertion dans un corps comprend un tube creux configuré de manière à entrer dans un corps et un revêtement couplé à au moins une partie du tube creux. Le revêtement comprend un lubrifiant qui est biocompatible et est soluble dans un solvant et un solvant comprenant lun parmi un hydrocarbure aliphatique, un hydrocarbure aromatique et un solvant chloré.