To provide a deodorization material small in detachment rate of adsorbed acetaldehyde when stood under high temperature atmosphere after adsorbing acetaldehyde.SOLUTION: There is provided a deodorization material containing active charcoal and (A) aromatic amine or sulfate of the aromatic amine or (B) aromatic amine, sulfate of the aromatic amine and sulfuric acid carried on the active charcoal, and having all pore volume of the active charcoal of 0.45 cc/g or more, total carried amount of the aromatic amine and the sulfate of the aromatic amine of 20 to 32 pts.mass based on 100 pts.mass of the active charcoal, and total carried amount of the sulfate of the aromatic amine and the sulfuric acid of 1.8 to 3.5 pts.mass based on 100 pts.mass of the active charcoal.SELECTED DRAWING: None【課題】アセトアルデヒドを吸着させた後に高温雰囲気下に置いたときの、吸着したアセトアルデヒドの脱離率の小さい脱臭材を提供する。【解決手段】活性炭と、前記活性炭に担持された、(A)芳香族アミン及び該芳香族アミンの硫酸塩、又は、(B)芳香族アミン、該芳香族アミンの硫酸塩、及び硫酸とを含む、脱臭材であって、 前記活性炭の全細孔容積が0.45cc/g以上であり、 前記活性炭100質量部に対する、前記芳香族アミンと前記芳香族アミンの硫酸塩との合計担持量が20~32質量部であり、 前記活性炭100質量部に対する、前記芳香族アミンの硫酸塩と前記硫酸との合計担持量が1.8~3.5質量部である、 脱臭材。【選択図】 なし