Articles with enhanced tensile strength and comfort are prepared from a latex comprising water and a styrenic block copolymer, wherein the styrenic block copolymer has 2 or more poly(vinyl aromatic) blocks and at least one block of polymerized conjugated diene, wherein the styrenic block copolymer has a weight average molecular weight of 150,000 to 250,000, the poly(vinyl aromatic) blocks have a weight average molecular weight ranging from 9,000 to 15,000, and the content of poly(vinylaromatic) blocks in the styrenic block copolymer ranges from 8 to 15% wt, based on the total styrenic block copolymer, by a process which comprises coating a surface with the latex to obtain a film, wherein the latex comprises a vulcanizing agent. The invention also provides a latex comprising such a styrenic block copolymer and a vulcanizing agent, as well as a styrenic block copolymer that is particularly suitable for use in such a latex.