PROBLEM TO BE SOLVED: To provide an advantageous method for forming a physiologically active surface on a balloon of a balloon catheter.SOLUTION: The method for forming a physiologically active surface on a balloon (3) of a balloon catheter (1) is described, where the surface of the balloon (3) is at least partially moistened with a first solution (8) of an active material, and a part of the surface of the balloon (3) moistened with the first solution (8) of the active material is moistened with a second saturation solution (28) of the active material. A balloon (3) of a balloon catheter (1), the surface of which includes at least partially a coated part with an active material (11) is described, where the coated part (11) is homogeneously and brittlely configured in an area where the whole thereof is coated.COPYRIGHT: (C)2015,JPO&INPIT【課題】バルーンカテーテルのバルーン上に生理活性表面を形成する有利な方法を提供する。【解決手段】バルーンカテーテル(1)のバルーン(3)上に生理活性表面を形成する方法が記載され、ここでは、バルーン(3)の表面が少なくとも部分的に、作用物質の第1の溶液(8)により湿らされ、作用物質の第1の溶液(8)により湿らされたバルーン(3)の表面の部分が、作用物質の第2の飽和溶液(28)により湿らされる。その表面が少なくとも部分的に作用物質(11)による被覆部を有する、バルーンカテーテル(1)のバルーン(3)が記載され、ここで被覆部(11)は全体が被覆された領域内で均質かつ脆性に構成されている。【選択図】図8