Problem to be solved: to provide a surface treatment agent having antiviral and excellent transparency which does not damage the appearance of the coating material when it is coated with antiviral.Solution comprising a paint containing an antiviral agent which is a calcium carbonate carrying a sulfonic acid surfactantThe coating is an antiviral surface treatment agent which is an ultraviolet curable paint or an electron beam hardened paint;A sulfonic acid based surfactant is made up of a coating containing an antiviral agent, an inorganic filler.The paint is an antiviral surface treatment agent which is an anionic aqueous resin emulsion;A sulfonic acid based surfactant is made up of a coating containing an antiviral agent, an inorganic filler.The paint is an aqueous resin emulsion or an organic solvent type paint;The antiviral surface treatment agent having a weight ratio of B: C of 1:5 to 1:1 is obtained from the sulfonic acid based surfactant (b) of the antiviral agent and the inorganic filler (c).No selection【課題】抗ウイルス性を有するとともに塗工された際に被塗工体の外観を損ねることがない、抗ウイルス性に優れ透明性を有する表面処理剤を提供する。【解決手段】スルホン酸系界面活性剤が担持された炭酸カルシウムである抗ウイルス剤を含有する塗料からなり、前記塗料が紫外線硬化型塗料または電子線硬化型塗料である抗ウイルス性表面処理剤であり、スルホン酸系界面活性剤が担持された無機充填剤である抗ウイルス剤を含有する塗料からなり、前記塗料がアニオン性の水性樹脂エマルジョンである抗ウイルス性表面処理剤であり、スルホン酸系界面活性剤が担持された無機充填剤である抗ウイルス剤を含有する塗料からなり、前記塗料が水性樹脂エマルジョンまたは有機溶剤系塗料であり、前記抗ウイルス剤のスルホン酸系界面活性剤(B)と無機充填剤(C)との重量比B:Cが1:5~1:1である抗ウイルス性表面処理剤である。【選択図】 なし