G8 INTERNATIONAL TRADING CO LTD;G-8 INTERNATIONAL TRADING 株式会社
发明人:
MATSUI SABURO,松井 三郎
申请号:
JP2018012267
公开号:
JP2019129710A
申请日:
2018.01.29
申请国别(地区):
JP
年份:
2019
代理人:
摘要:
To provide a method for manufacturing fulvic acid iron for manufacturing it efficiently and in a short time.SOLUTION: A manufacturing method includes: a device preparation step for preparing a processing unit equipped with a sealed container 12 that can be closed, steam jetting means 14 for jetting high-temperature and high-pressure steam into the sealed container 12, a supply part for supplying a raw material, and a discharge part for discharging processing liquid generated by the processing of the raw material by steam to the outside; a raw material feeding step for feeding a woody plant material (and/or a herb material) and iron hydroxide into the sealed container 12 of the processing unit from the supply part as main raw materials; a processing step for introducing steam with a temperature of 120-250°C and a pressure of 2-35 atm in the woody plant material, and steam with a temperature of 100-200°C and a pressure of 2-25 atm in the herb material to the processing space, subjecting the raw materials to a subcritical water reaction treatment while agitating the raw materials, and acquiring a mixed solution containing fulvic acid iron hydroxide; and a fulvic acid iron hydroxide solution acquisition step for separating fulvic acid iron hydroxide from the acquired mixed solution, and acquiring a fulvic acid iron solution.SELECTED DRAWING: Figure 1【課題】フルボ酸鉄を効率よく短時間で製造することのできるフルボ酸鉄の製造方法を提供する。【解決手段】製造方法は、閉鎖可能な密閉容器12と、密閉容器12内に高温高圧の蒸気を噴出する蒸気噴出手段14と、原料を供給する供給部と、蒸気による原料の処理により生成された処理液を外部に排出する排出部とを備えた処理装置を準備する装置準備工程、前期処理装置の密閉容器12内に、前期供給部から木本材(及び/又は草本材)と水酸化鉄を主原料として投入する原料投入工程、木本材は温度が120~250℃で圧力が2~35atmの蒸気を、草本材は100~200℃で圧力が2~25atmの蒸気を前記処理空間内に導入し、原料を撹拌しながら原料を亜臨界水反応処理して、フルボ酸水酸化鉄を含有する混合溶液を得る処理工程、及び取得した混合溶液からフルボ酸水酸化鉄を分離して、フルボ酸鉄溶液を取得するフルボ酸水酸化鉄溶液取得工程を備えている。【選択図】図1