A zirconium alloy nuclear reactor cylindrical cladding has an inner Zr substrate surface (10), an outer volume of protective material (22), and an integrated middle volume (20) of zirconium oxide, zirconium and protective material, where the protective material is applied by impaction at a velocity greater than 340 meters/second to provide the integrated middle volume (20) resulting in structural integrity for the cladding.