The present invention relates to a process allowing the production of a high molar mass homogeneous polymer. The method comprises the steps of: a) providing a first liquid reaction mixture comprising a cyclic imino ether monomer and optionally a solvent; b) polymerizing the cyclic imino ether monomer by cationic ring-opening polymerization; and (i) a polymer. And (ii) producing a polymerized first reaction mixture containing a solvent and / or unreacted cyclic iminoether monomer, c) separating the solvent and / or unreacted cyclic iminoether monomer from the polymer D) providing a second liquid reaction mixture containing the cyclic iminoether monomer and solvent by combining the separated unreacted cyclic iminoether monomer and / or the separated solvent with other ingredients. And e) a cyclic iminoether monomer in the second reaction mixture by cationic ring-opening polymerization. The comprises the step of polymerizing. [Selection figure] None本発明は、高モル質量の均一なポリマーの製造を可能にする方法に関する。この方法は、a)環状イミノエーテルモノマー及び任意選択で溶媒を含む、第1の液体反応混合物を用意するステップ、b)カチオン開環重合によって環状イミノエーテルモノマーを重合して、(i)重合物及び(ii)溶媒及び/又は未反応の環状イミノエーテルモノマーを含有する、重合した第1の反応混合物を生成するステップ、c)重合物から、溶媒及び/又は未反応の環状イミノエーテルモノマーを分離するステップ、d)分離された未反応の環状イミノエーテルモノマー及び/又は分離された溶媒を、その他の成分と組み合わせることによって、環状イミノエーテルモノマー及び溶媒を含有する、第2の液体反応混合物を用意するステップ、並びにe)カチオン開環重合によって第2の反応混合物中で環状イミノエーテルモノマーを重合するステップを含む。【選択図】なし