Federalnoe Gosudarstvennoe byudzhetnoe nauchnoe uchrezhdenie "Federalnyj nauchnyj tsentr biologicheskikh sistem i agrotekhnologij rossijskoj akademii nauk"
发明人:
Galiev Bulat Khabuleevich (RU),Галиев Булат Хабулеевич (RU),Shirnina Nadezhda Mikhajlovna (RU),Ширнина Надежда Михайловна (RU),Miroshnikov Ivan Sergeevich (RU),Мирошников Иван Сергеевич (RU),Makaeva A
申请号:
RU2019103614
公开号:
RU0002706572C1
申请日:
2019.02.08
申请国别(地区):
RU
年份:
2019
代理人:
摘要:
FIELD: agriculture.SUBSTANCE: invention relates to agriculture, in particular to fodder production. Method for preparation of concentrated feed mixture for cattle, including mixing wheat bran, milled grain fodder, mineral additive, and a premix with a solution of alkaline electrochemically activated cathode water with pH 9–9.5 and redox potential of -400…-500 mV stabilized with glycine in amount of 0.5 wt% in ratio 1:2. Further, the mixture is subjected to ultrasonic cavitation treatment at frequency of 30 kHz with exposure of 30 minutes at 35 °C. Premix contains 142 mg of zinc oxide, 188 mg of manganese carbonate, 68 mg of copper sulphate, 2 mg of potassium iodide, 5 mg of FeCo alloy nanoparticles with size of 62.5 nm, 6.6 g of sulfur, and the mineral additive consists of monosodium phosphate , fodder chalk and table salt. Initial components of the concentrated fodder mixture are used at the following ratio, wt%: wheat offal – 57, milled grain fodder – 40, monosodium phosphate – 0.3, fodder chalk – 0.7, culinary salt – 1.0, premix – 1.0. Obtained concentrated mixture is dosed into the ration of young cattle fattened in amount of 45–50 % of the daily ration value.EFFECT: proposed method for preparation of fodder mixture ensures production of product increasing efficiency of cattle.1 cl, 2 tblИзобретение относится к отрасли сельского хозяйства, в частности к кормопроизводству. Способ приготовления концентрированной кормовой смеси для крупного рогатого скота, включающий смешивание пшеничных отрубей, измельченного зернового корма, минеральной добавки, и премикса с раствором щелочной электрохимически активированной катодной воды с рН 9-9,5 и редокспотенциалом -400…-500 мВ, стабилизированной глицином в количестве 0,5 мас. %, в соотношении 1:2. Далее осуществляют ультразвуковую кавитационную обработку смеси частотой 30 кГц с экспозицией 30 мин при температуре 35°С. При этом премикс содержит 142 мг окиси цинка, 188 мг углекислого марганца, 68 мг сернокислой меди, 2 мг йоди