PROBLEM TO BE SOLVED: To provide a manufacturing method of a wired ring having excellent joining strength at a distal end of a wire with respect to a ring member, a manufacturing method of distal-deflecting movable catheter including the wired ring, and a jig for manufacturing the wired ring.SOLUTION: A silver brazing material 36 is attached to distal ends 30a and 31a of a first wire 30 and a second wire 31 projecting from a ring 32. Then, the wires 30 and 31 are axially moved along fitting grooves 44 and 45, and the distal ends 30a and 31a of the wires 30 and 31 to which the silver brazing material 36 is attached are drawn inside the ring 32, and brought into contact with the inner peripheral surface of the ring 32 respectively via the silver brazing material 36. The ring 32 is heated with it coming into contact with the distal ends, to melt the silver brazing material 36, so that the distal ends 30a and 31a of the first wire 30 and the second wire 31 are simultaneously joined with the ring 32 respectively.COPYRIGHT: (C)2015,JPO&INPIT【課題】リング部材に対するワイヤの遠位端の接合強度に優れたワイヤ付きリングの製造方法、そのワイヤ付きリングを有する先端偏向可動カテーテルの製造方法およびワイヤ付きリングの製造用治具を提供すること。【解決手段】リング32から飛び出している第1ワイヤ30および第2ワイヤ31の遠位端30a,31aに、銀ロウ材36を付着させる。次に、取付溝44,45に沿ってワイヤ30,31を軸方向に移動させ、銀ロウ材36が付着してあるワイヤ30,31の遠位端30a,31aを、リング32の内部に引き込み、それぞれリング32の内周面に銀ロウ材36を介して接触させる。その状態でリング32を加熱して銀ロウ材36を熔融させ、第1ワイヤ30および第2ワイヤ31の遠位端30a,31aをそれぞれリング32に同時に接合する。【選択図】図10