I order to obtain the orthopedic fixation materials of photo-curable by visible light, the resulting strength required in a short time. Providing a photocurable resin containing a photoinitiator which absorbs light 400~700nm and urethane (meth) acrylate oligomer of the formula I. And a support member 5 and is held by the substrate 3 and the light-curable resin 4. 6 cushions inside of the support member 5, is covered with a cover material 2 outside, to obtain a splint material 1 is orthopedic fixation material. And applied to the affected area a cushioning material 6 side, to the molding while irradiating visible light bandaged from above. Sprint is able to cure progresses, I can fix the affected area. (Formula I, A is. Shown having a hydroxyl group, each (meth) acrylate residues diisocyanate residue, X, is Y)可視光線により、短時間で必要な強度が得られる光硬化型の整形外科用固定材を得ようとする。式Iのウレタン(メタ)アクリレートオリゴマーと400~700nmの光を吸収する光重合開始剤を含む光硬化型樹脂を用意する。この光硬化型樹脂4を基材3に保持させて支持材5とする。この支持材5の内側を緩衝材6で、外側をカバー材2で覆い、整形外科用固定材であるスプリント材1を得る。緩衝材6側を患部に当て、その上から包帯を巻いて可視光を照射しながらモールディングをする。硬化が進むとスプリントが出来て、患部を固定できる。(式I中、Aはジイソシアネート残基、X,Yは各々ヒドロキシル基を有する(メタ)アクリレート残基を示す。)