PROBLEM TO BE SOLVED: To obtain a liquid metal target with high durability capable of restraining boiling of liquid metal.SOLUTION: A liquid metal target 100 is provided with a first ferromagnetic rib 15 projecting downward on a rear side of an emission nozzle 12 of a first structure 10. Also, a second ferromagnetic rib 25 projecting upward on a rear side of a receiving nozzle 22 of a second structure 20 is provided vertically symmetrical to the first ferromagnetic rib. In such a structure, a shape of a magnetic force line varies so that a magnetic force line is directed to a vertical direction at portions where the first ferromagnetic rib 15 and the second ferromagnetic rib 25 are provided in a horizontal direction. Therefore, the magnetic force line in front of the portions and under the emission nozzle 12 can be curved forward. Thereby, a liquid lithium flow passage C can be curved forward.COPYRIGHT: (C)2015,JPO&INPIT【課題】液体金属の沸騰を抑制し、かつ耐久性が高い液体金属ターゲットを得る。【解決手段】この液体金属ターゲット100においては、第1構造体10の発射ノズル12の後方側において下向きに突出する第1強磁性体リブ15が設けられている。また、これと上下対称に、 第2構造体20の受容ノズル22の後方側において上向きに突出する第2強磁性体リブ25が設けられている。この構成においては、水平方向において、第1強磁性体リブ15、第2強磁性体リブ25が設けられた箇所において磁力線が鉛直方向を向くように、磁力線の形状が変化する。このため、この箇所よりも前方となる発射ノズル12下の磁力線を前方に湾曲させることができる。これにより、液体リチウム流路Cを前方に湾曲させることができる。【選択図】図7