PROBLEM TO BE SOLVED: To provide a method for producing a tablet that maintains a tablet shape after production, has no emission of carbon dioxide gas by storage, has excellent foaming properties when used and comprises a dissolvable component that is quickly dissolved in water.SOLUTION: In the method for producing a tablet in which the powder temperature of sodium hydrogen carbonate is raised to 50-68°C by using a granulator, sodium hydrogen carbonate is mixed with 1-15% of polyethylene glycol and granulated, the granule is cooled to give a granule A which is stirred and mixed with citric acid or a citric acid polyethylene granule B and an anhydride and compression molded, the granule A of sodium hydrogen carbonate is mixed with citric acid or the citric acid granule B in the ratio of 2:1 to 10:1 and, in any process before compression molding, an anhydride selected from sodium carbonate, calcium carbonate and magnesium carbonate in an amount of 1/10 to 1/100 of the amount of sodium hydrogen carbonate and compression molded.COPYRIGHT: (C)2013,JPO&INPIT【課題】製造後、錠剤の形状を維持し、保存による炭酸ガスの発生も無く、使用に際し良好な発泡性を有し、溶解可能な成分は速やかに水に溶解する錠剤の製造方法の提供。【解決手段】炭酸水素ナトリウムを造粒機を用いて粉体温度を50~68℃に上げ、炭酸水素ナトリウムに対して1~15%のポリエチレングリコールを添加して造粒し、この造粒物を冷却して得た造粒物Aと、クエン酸、もしくはクエン酸のポリエチレン造粒物B及び無水物を撹拌、混合して、圧縮成型によって錠剤を製造する方法において、炭酸水素ナトリウムの造粒物A対クエン酸もしくはクエン酸造粒物Bが、2対1~10対1の比率となるように添加し、さらに、圧縮成型前のいずれかの工程において、炭酸水素ナトリウムの1/10から1/100の量の、炭酸ナトリウム、炭酸カルシウム、炭酸マグネシウムから選ばれる無水物を添加し含有させて混合して圧縮成型する錠剤の製造方法。【選択図】なし