摘要:
The present invention relates to sustained release of the bone-forming ions, and to provide a high bone repair material with excellent safety in apatite-forming ability and storage stability. A first aqueous solution of the alkaline containing one or more cations of the A calcium ions and sodium ions and potassium ions containing no bone-forming ions, immersing a substrate made of titanium or a titanium alloy drying a step, calcium ions, and strontium, magnesium, zinc, immersing the substrate in a second aqueous solution comprising an osteogenic ion is one or more selected from the ions of lithium and gallium, the substrate to be characterized in that it comprises a step of heating in an atmosphere, water, a step of immersion in a third aqueous solution comprising one or more selected from among aqueous acid solution and bone-forming ions containing aqueous solution.【課題】骨形成イオンを徐放し、且つアパタイト形成能及び保存性に優れた安全性の高い骨修復材料を提供する。【解決手段】カルシウムイオン及び骨形成イオンを含まずナトリウムイオン及びカリウムイオンのうち1つ以上の陽イオンを含むアルカリ性の第1の水溶液に、チタンまたはチタン合金からなる基材を浸漬する工程と、カルシウムイオン、並びにストロンチウム、マグネシウム、亜鉛、リチウム及びガリウムのイオンから選択される1つ以上である骨形成イオンを含む第2の水溶液に基材を浸漬する工程と、基材を乾燥雰囲気中で加熱する工程と、水、酸水溶液及び骨形成イオン含有水溶液のうちから選ばれる1種以上からなる第3の水溶液に浸漬する工程を備えることを特徴とする。
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充