PROBLEM TO BE SOLVED: To provide a ceramic thin film which accelerates bone formation by its bone induction ability which is more excellent than the conventional hydroxyapatite and strontium-substituted apatite, and can improve its sticking or adhesion with gnathic bone and cells, and to provide a bone tissue implant having the thin film as a coating layer and a method for producing the same.SOLUTION: Provided is a phosphate type ceramic thin film containing a bone formation accelerator, including at least one element selected from the group consisting of strontium, magnesium, and zinc as the bone formation accelerator. The ceramic thin film contains the element included as the bone formation accelerator in an amount exceeding 20 atomic%, more preferably in a range of 40 to 80 atomic%, relative to an amount of all elements constituting cations of the phosphate type ceramic thin film. Further, a remaining element to constitute the cations is calcium.COPYRIGHT: (C)2015,JPO&INPIT【課題】従来のハイドロキシアパタイトやストロンチウム置換アパタイトよりも優れた骨誘導能によって骨形成を促進させ、顎骨及び細胞との付着又は接着を向上することができるセラミック薄膜及び該薄膜を被覆層として有する骨組織インプラント及びその製造方法を提供する。【解決する手段】本発明による骨形成促進物質含有のリン酸塩セラミック薄膜は、骨形成促進物質としてストロンチウム、マグネシウム及び亜鉛からなる群の少なくとも1つの元素を含むリン酸塩型セラミック薄膜であって、骨形成促進物質として含まれる前記元素を、前記リン酸塩型セラミック薄膜のカチオンを構成する全元素量に対して20原子%を超えて、さらに好ましくは40~80原子%の範囲で含有し、且つ、前記カチオンを構成する残余の元素がカルシウムであることを特徴とする。【選択図】図2
来源网站:
中国工程科技知识中心
来源网址:
http://www.ckcest.cn/home/

意 见 箱

匿名:登录

个人用户登录

找回密码

第三方账号登录

忘记密码

个人用户注册

必须为有效邮箱
6~16位数字与字母组合
6~16位数字与字母组合
请输入正确的手机号码

信息补充