The present invention relates to a method for obtaining electrolysed water comprising the following steps: - Providing running or spring water, optionally comprising sodium chloride (NaCl) at a concentration of 0.5 to 2g/L - Electrolysing this water by means of an electrolysis module comprising at least one boron-doped diamond electrode attached to a silicon substrate in which the concentration of boron is between 200 ppm (3x1019 B atoms/cm3) and 1500 ppm (2x1020 B atoms/cm3), the electric current density during the electrolysis process being between 15 and 500 mAh/L water, more preferably between 40 and 250 mAh/L water, and more preferably still between 50 and 200 mAh/L, and the electrolysis period being less than or equal to 60 minutes. The invention also concerns a water obtained according to this method for treating skin disorders and a composition containing such a water and a device for treating skin disorders comprising a vessel containing a water obtained according to the inventive method.La présente invention concerne un procédé d'obtention d'une eau électrolysée comportant les étapes suivantes : - Procuration d'une eau courante ou de source, comprenant optionnellement du chlorure de sodium (NaCl) à la concentration 0,5 à 2g/L - Electrolyse de ladite eau par un module d'électrolyse comprenant au moins une électrode de diamant dopée au bore fixée sur substrat de silicium dans laquelle la concentration de bore est comprise entre 200 ppm (3x1019 B atomes/cm3) et 1500 ppm (2x1020 B atomes/cm3), la densité de courant électrique lors du processus d'électrolyse étant comprise entre et 500 mAh/L d'eau, plus préférentiellement 40 à 250 mAh/L d'eau, encore plus préférentiellement 50 à 200 mAh/L, et la durée d'électrolyse étant inférieure ou égale à 60 minutes. L'invention concerne par ailleurs une eau obtenue selon ce procédé pour le traitement d'affections de la peau ainsi qu'une composition contenant une telle eau et un dispositif de traitement des affections de la