A chewing gum base is disclosed comprising a solution polymerized styrene-butadiene rubber having (i) a glass transition temperature Tg ranging from -20 °C to 0 °C and/or (ii) an intersection of G' with G" at a frequency between 100 and 105 rad/sec at 30 °C and 1% strain as measured following ASTM D4440-08.