Provided are a method for manufacturing a mask pack for heavy metal adsorption comprising immersing a cellulose nonwoven fabric in an alkali solution by a cold pad batch method and then aging the cellulose nonwoven fabric at room temperature for 10 minutes to 50 minutes, and immersing the cellulose nonwoven fabric in a carboxymethylation solution by the cold pad batch method and then aging the cellulose nonwoven fabric at room temperature to 60°C for 10 minutes to 3 hours, and a mask pack for heavy metal adsorption manufactured by the method.